Charpy Impact 191 - 212 J
141 - 156 ft-lb
ATI Allegheny Ludlum Alloy 255 Stainless Steel, UNS S32550
Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applicatio..