Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 244 J
180 ft-lb
Typical; machined from plate
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The al..