Material Notes:
Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The alloy is used in a variety of corrosion resisting applications. The high nickel content of the alloy provides a level of resistance to reducing environments, while the chromium content of the material provides resistance to weaker oxidizing environments. The high nickel content of the material provides exceptional resistance to chloride stress corrosion cracking. The forming properties are similar to those of stable austenitic stainless steels. Specific uses include furnace parts, heat treatment fixtures, chemical and food processing, and nuclear reactors.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.42 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Typical Annealed
Tensile Strength, Ultimate 640 MPa
92800 psi
Typical Annealed
Tensile Strength, Yield 255 MPa

@Strain 0.200 %
37000 psi

@Strain 0.200 %
Typical; Annealed
Elongation at Break 45 %
45 %
typical in 2"; Annealed
Modulus of Elasticity 207 GPa
30000 ksi
Poissons Ratio 0.29
0.29
Shear Modulus 76.0 GPa
11000 ksi
Charpy Impact 244 J
180 ft-lb
Typical; machined from plate
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 20.0 - 93.0 °C
6.89 µin/in-°F

@Temperature 68.0 - 199 °F
13.7 µm/m-°C

@Temperature 20.0 - 315 °C
7.61 µin/in-°F

@Temperature 68.0 - 599 °F
14.6 µm/m-°C

@Temperature 20.0 - 538 °C
8.11 µin/in-°F

@Temperature 68.0 - 1000 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 14.8 W/m-K
103 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 15.5 %
15.5 %
Copper, Cu 0.10 %
0.10 %
Iron, Fe 8.0 %
8.0 %
Manganese, Mn 0.25 %
0.25 %
Nickel, Ni 76 %
76 %
as balance; includes Co
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0020 %
0.0020 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.02
<= 1.02