Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 155 J | 114 ft-lb | V Notch; plate |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Charpy Impact | 155 J @Temperature 177 °C |
114 ft-lb @Temperature 351 °F |
V-notch |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |