Polymer Property : Charpy Impact = 1.3 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 1.7 J

@Temperature -35.0 °C
1.3 ft-lb

@Temperature -31.0 °F
Notched
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..