Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 495 MPa @# of Cycles 2.00e+6 |
<= 71800 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Fatigue Strength | <= 495 MPa @# of Cycles 1.00e+7 |
<= 71800 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |