Mechanical Properties Metric English Comments
Fatigue Strength <= 495 MPa

@# of Cycles 2.00e+6
<= 71800 psi

@# of Cycles 2.00e+6
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r..
Fatigue Strength <= 495 MPa

@# of Cycles 1.00e+7
<= 71800 psi

@# of Cycles 1.00e+7
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r..