Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 480 MPa @# of Cycles 100000 |
<= 69600 psi @# of Cycles 100000 |
|
ArcelorMittal HSLA 420 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC420LA), electroglavanized (HC420LA +ZE) and Extragal®/galfan/Galvannealed (HC420LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |
|||
Fatigue Strength | <= 480 MPa @# of Cycles 100000 |
<= 69600 psi @# of Cycles 100000 |
|
ArcelorMittal FB 540 Hot rolled ferrite-bainite steel Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steel.. |