Mechanical Properties Metric English Comments
Fatigue Strength 370 MPa

@# of Cycles 1.00e+7
53700 psi

@# of Cycles 1.00e+7
Rod, rotating bend
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed
Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi..