Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 295 MPa @# of Cycles 100000 |
<= 42800 psi @# of Cycles 100000 |
|
ArcelorMittal H 220 Solid solution steel, Cold rolled Available in the following: uncoated (HC220P) and electrogalvanized (HC220P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |