Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 278 MPa @# of Cycles 1.00e+7 |
40300 psi @# of Cycles 1.00e+7 |
Smooth, Kt=1; rotating bend (sample with UTS = 589 Mpa) |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |