Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 232 MPa @# of Cycles 1.00e+7 |
33600 psi @# of Cycles 1.00e+7 |
Smooth, Kt=1; rotating bend |
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2) Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,.. |