Fatigue Strength 116 MPa

@# of Cycles 1.00e+7
16800 psi

@# of Cycles 1.00e+7
Notched, Kt=4; rotating bend (sample with UTS = 589 MPa)
TIMET CP Titanium (ASTM Grade 3)
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti..
Fatigue Strength 116 MPa

@# of Cycles 1.00e+7
16800 psi

@# of Cycles 1.00e+7
Notched, Kt=3.3; rotating bend (sample with UTS = 550 MPa)
TIMET CP Titanium (ASTM Grade 3)
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti..