Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 97.0 GPa | 14100 ksi | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Modulus of Elasticity | 97.0 GPa | 14100 ksi | |
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |