Mechanical Properties Metric English Comments
Modulus of Elasticity 97.0 GPa
14100 ksi
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th..
Modulus of Elasticity 97.0 GPa
14100 ksi
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th..