Polymer Property : Modulus of Elasticity = 914 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 6.30 GPa
914 ksi
ISO 527-2
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 6.30 GPa
914 ksi
Conditioned; ISO 178
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
Modulus of Elasticity 6.30 GPa
914 ksi
ASTM D638
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass
Polyphenylene Oxide provides excellent resistance to aqueous media. It is softened by aromatic hydrocarbons. Data provided by the manufacturer, Owens Corning.
Modulus of Elasticity 6.30 - 25.1 GPa
914 - 3640 ksi
Average value: 14.1 GPa Grade Count:16
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..