Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 627 GPa | 90900 ksi | |
CoorsTek ACI-Co6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Modulus of Elasticity | 627 GPa | 90900 ksi | ASTM C848 |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |