Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 8.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 178
Addiplast Addinyl A2 V30 Nylon 66, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 527
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade.
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 178
Addiplast Addinyl A2 ZV30 Nylon 66, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 527-2
BASF Ultradur B 4406 G4 PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Modulus of Elasticity 8.20 - 23.0 GPa

@Temperature 60.0 - 150 °C
1190 - 3340 ksi

@Temperature 140 - 302 °F
Average value: 14.6 GPa Grade Count:1
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 178
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 8.20 GPa
1190 ksi
ISO 178
Addiplast Addinyl B2 ZV30 Nylon 6, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Copyright © lookpolymers.com All Rights Reserved