Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.50 - 8.10 GPa @Temperature 40.0 - 140 °C |
363 - 1170 ksi @Temperature 104 - 284 °F |
Average value: 5.10 GPa Grade Count:2 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |