Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0483 GPa
7.00 ksi
Arlon SQA-TMS-008
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr..