Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Carrier
381 microns
15.0 mil
Product; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
Silicone Property; ASTM D2240
Tensile Strength 4.41 MPa
640 psi
Silicone Property; ASTM D412
Elongation at Break 15 %
15 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.0483 GPa
7.00 ksi
Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
Shear Modulus <= 0.000483 GPa
<= 0.0700 ksi
Arlon SQA-TMS-018
Shear Strength 2.41 MPa
350 psi
Lap; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
ASTM E831
Specific Heat Capacity 0.760 J/g-°C
0.182 BTU/lb-°F
E1461-01
Thermal Conductivity 1.20 W/m-K
8.33 BTU-in/hr-ft²-°F
ASTM E1530
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -116 °C
-177 °F
ASTM E1356
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IPC TM 650 - 2.5.5.3
Dielectric Strength 39.4 kV/mm
1000 kV/in
ASTM D149
Dissipation Factor 0.0015

@Frequency 1.00e+6 Hz
0.0015

@Frequency 1.00e+6 Hz
IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 121 °C
0.250 hour

@Temperature 250 °F
Recommended Cure Cycle; Under Pressure
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color White
Thermal Resistance (°C-in2/W) 0.5
ASTM E1530
Total Product Weight (oz/yd2) 19
Arlon SQA-TMS-025