Polymer Property : Modulus of Elasticity = 62.1 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 27.6 - 62.1 GPa
4000 - 9000 ksi
Sonic Modulus
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..