Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 27.6 - 62.1 GPa | 4000 - 9000 ksi | Sonic Modulus |
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Modulus of Elasticity | 27.6 GPa | 4000 ksi | |
Indium Corp. Indalloy 226 Tin Solder Alloy Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 27.6 GPa | 4000 ksi | IPC TM-650 2.4.18.3 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Modulus of Elasticity | 27.6 GPa | 4000 ksi | IPC TM-650 2.4.18.3 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |