Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.86 GPa | 560 ksi | IPC TM-650 2.4.18.3 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |