Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.86 GPa | 560 ksi | IPC TM-650 2.4.18.3 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Modulus of Elasticity | 3.86 - 39.7 GPa | 561 - 5760 ksi | Average value: 11.1 GPa Grade Count:156 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |