Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 370 GPa | 53700 ksi | |
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | |
H.C. Starck HPM 1810 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | ASTM C848 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | ASTM-C848 |
CoorsTek AD-996 99.6% Alumina |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | ASTM C848 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | ASTM-C848 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | ASTM C848 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 370 GPa | 53700 ksi | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |