Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 5200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 35.9 GPa
5200 ksi
Carlisle 201HD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Modulus of Elasticity 35.9 GPa
5200 ksi
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Modulus of Elasticity 35.9 GPa
5200 ksi
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Modulus of Elasticity 35.9 GPa
5200 ksi
Carlisle 201LD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Copyright © lookpolymers.com All Rights Reserved