Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0379 GPa | 5.50 ksi | ISO R527 |
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |