Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D1505
Vinyl Acetate Content 17 - 20 %
17 - 20 %
Melt Flow 6.0 - 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 30.5
30.5
ISO 868
Tensile Strength at Break 24.0 MPa
3480 psi
50 microns film; ASTM D882
Tensile Strength, Yield 5.40 MPa
783 psi
50 microns film; ASTM D882
Elongation at Break 695 %
695 %
50 microns film; ASTM D882
Modulus of Elasticity 0.0379 GPa
5.50 ksi
ISO R527
Dart Drop Test 250 g
0.551 lb
50 microns film
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
D.S.C. method
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.3 %
6.3 %
50 micron film; ASTM D1003