Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
Modulus of Elasticity | 2.69 - 5.50 GPa | 390 - 798 ksi | Average value: 3.34 GPa Grade Count:6 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |