Mechanical Properties Metric English Comments
Modulus of Elasticity 335 GPa
48600 ksi
DIN V ENV 843-2
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua..