Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 335 GPa | 48600 ksi | DIN V ENV 843-2 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |