Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 32.5 GPa | 4710 ksi | |
California Fine Wire Alloy 411 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |