Polymer Property : Modulus of Elasticity = 462 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.19 GPa
462 ksi
Cross; ASTM D638
Arlon CLTE-P Pre-Preg Bonding Layer
Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of ..