Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00163 - 3.14966 GPa

@Temperature -100 - 200 °C
0.236 - 456.827 ksi

@Temperature -148 - 392 °F
Average value: 0.685 GPa Grade Count:20
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..