Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00163 - 3.14966 GPa @Temperature -100 - 200 °C |
0.236 - 456.827 ksi @Temperature -148 - 392 °F |
Average value: 0.685 GPa Grade Count:20 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 0.00163 GPa | 0.237 ksi | ASTM D638 |
Colorite Polymers Elastichem 3511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Modulus of Elasticity | 0.00163 GPa | 0.237 ksi | After 7 days at 100°C; ASTM D412 ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Modulus of Elasticity | 0.00163 - 3.24 GPa | 0.237 - 470 ksi | Average value: 2.12 GPa Grade Count:55 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |