Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.30 - 30.9 GPa | 189 - 4480 ksi | Average value: 11.1 GPa Grade Count:218 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |