Polymer Property : Modulus of Elasticity = 44.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 44.0 GPa
6380 ksi
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..