Polymer Property : Modulus of Elasticity = 4200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.50 - 29.0 GPa
653 - 4200 ksi
Average value: 16.5 GPa Grade Count:8
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 1.60 - 29.0 GPa
232 - 4200 ksi
Average value: 8.94 GPa Grade Count:55
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..