Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.320 - 4.09 GPa @Temperature -40.0 - 150 °C |
46.4 - 593 ksi @Temperature -40.0 - 302 °F |
Average value: 1.17 GPa Grade Count:8 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |