Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.70 - 2.70 GPa | 247 - 392 ksi | Average value: 2.27 GPa Grade Count:50 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Modulus of Elasticity | 1.47 - 2.70 GPa | 213 - 392 ksi | Average value: 2.24 GPa Grade Count:44 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |