Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 246 GPa | 35700 ksi | |
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |