Mechanical Properties Metric English Comments
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 219 GPa

@Temperature 100 °C
31800 ksi

@Temperature 212 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Modulus of Elasticity 219 GPa

@Temperature 200 °C
31800 ksi

@Temperature 392 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Copyright © lookpolymers.com All Rights Reserved