Polymer Property : Modulus of Elasticity = 3.79 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.950 - 3.79 GPa
138 - 550 ksi
Average value: 2.89 GPa Grade Count:192
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Modulus of Elasticity 1.50 - 3.79 GPa
218 - 550 ksi
Average value: 2.57 GPa Grade Count:39
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Modulus of Elasticity 3.45 - 3.79 GPa
500 - 550 ksi
Average value: 3.55 GPa Grade Count:10
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an..