Polymer Property : Modulus of Elasticity = 3.47 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.47 GPa
503 ksi
ISO 527
GEHR Plastics PA 6 C Nylon 6 Cast
Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac..