Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-7327 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation. |
|||
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 19.0 GPa @Thickness >=1.50 mm |
2760 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |