Mechanical Properties Metric English Comments
Modulus of Elasticity 230 GPa
33400 ksi
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Modulus of Elasticity 230 GPa
33400 ksi
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
Modulus of Elasticity 230 GPa

@Temperature 200 °C
33400 ksi

@Temperature 392 °F
hardened to 58 HRC
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for..
Modulus of Elasticity 230 GPa
33400 ksi
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Modulus of Elasticity 230 GPa
33400 ksi
Bar
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Modulus of Elasticity 230 GPa
33400 ksi
Assab Steels ASP 23 Cold Work Steel
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope..