Mechanical Properties Metric English Comments
Modulus of Elasticity 1.566 GPa
227.1 ksi
ASTM D638
Huntsman Rexell® H2105 Injection Molding LLDPE  (discontinued **)
Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates..