Huntsman Rexell® H2105 Injection Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Rexell® H2105 Injection Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.aInformation provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Viscosity 81 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
81 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
185 cP

@Shear Rate 1000 1/s,
Temperature 230 °C
185 cP

@Shear Rate 1000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
304 cP

@Shear Rate 300 1/s,
Temperature 230 °C
304 cP

@Shear Rate 300 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Melt Flow 8.3 g/10 min
8.3 g/10 min
Melt Flow Ratio (I10/I2) is 7.2; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Modulus of Elasticity 1.566 GPa
227.1 ksi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
ASTM D1525