Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.140 - 1.57 GPa | 20.3 - 227 ksi | Average value: 0.441 GPa Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |